Automatic Twin-Jet Electropolisher for Thinning Tem Samples in Tem (Transmission electron microscope) Laboratory
Zhengzhou CY Technology Instrument Co., Ltd.
Fully Automatic Production Type Single Cavity Atomic Layer Deposition System
- Measurement method
- Vacuum gauge, Temperature controller
- Performance
- automatic, multi-function, wide application, High precision
- Country of origin
- China
- Delivery time
- Confirmed on request
Price on request
This supplier quotes prices based on quantity and delivery terms.
Product technical specifications
| Product name | Fully Automatic Production Type Single Cavity Atomic Layer Deposition System |
|---|---|
| Measurement method | Vacuum gauge, Temperature controller |
| Performance | automatic, multi-function, wide application, High precision |
| Standards | According to customer requirements, CE |
| Installation, Training and Setting-up | Video technical support, Online technical support, Product Manual |
| Color | Light blue |
| Warranty | 1Year |
| After Sale Services | lifetime |
| Country of origin | China |
| Sales unit | piece |
About Fully Automatic Production Type Single Cavity Atomic Layer Deposition System
Fully Automatic Production Type Single Cavity Atomic Layer Deposition System: Introduction of Atomic Layer Deposition System:
CY-KMT-500S Atomic Layer Deposition System I a fully automatic, productive, single-chamber system specially developed for middle-scale experiments of industrialization. Equipped with standard deposition process configuration, the system satisfies the demand of industry application.
Product benefit
Advanced software controlling system: many functions are integrated in the system, including technological formulation, parameter setting, popedom stetting ,interlocking alarming ad state supervisory control.
ALD Films
Elementary substance: Co, Cu, Ta, Ti, W, Ge, Pt, Ru, Ni, Fe…
Nitride: TiN, SiN, AlN, TaN, ZrN, HfN, WN …
Oxide: TiO2, HfO2, SiO2, ZnO, ZrO2, Al2O3, La2O3, SnO2…
Others: GaAs, AlP, InP, GaP, InAs, LaHfxOy, SrTiO3,SrTaO6…
Application fields of ALD
High-k gate oxides
Storage capacitor dielectrics
High aspect ratio diffusion barriers for Cu interconnects
Pinhole-free passivation layers for OLEDs and polymers
Highly conformal coatings for MEMS applications
Coating of nanoporous structures
Doping of special fiber
Solar battery
Flat plate display
Optical thin-film
Nano film of other special structure
Technical parameters of Atomic Layer Deposition System:
Wafer Dimension
8 inch and below
Wafer temperature
RT-500ºC,Controlling precision ±0.1ºC
Number of precursor
Two precursor lines, optional more lines
Temperature of precursor lines
RT-200ºC,Controlling precision ±0.1ºC
ALD Valve
Swagelok ALD swift valve
Background vacuum
<5*10-3Torr
Gas carrier system
N2 or Ar
Growing mode
Consecutive or interval deposition mode
Controlling system
PLC plus touch screen or display
Power supply
50-60Hz,380V/40A AC
Depositon Heterogeneity
Inside ship<±1%,between chip <±1.5%
Thoughput capacity
500 wafers of 8 inch
Process time
5 s/cycle
Dimension of the instrument
1400mmx800mmx2000mm
Recorded specifications
Measurement method: Vacuum gauge
Measurement method: Temperature controller
Performance: automatic
Standards: According to customer requirements
Installation, Training and Setting-up: Video technical support
Performance: multi-function
Standards: CE
Installation, Training and Setting-up: Online technical support
Supply terms
Request current pricing, availability, minimum order quantity and delivery time from the supplier.
- Payment through Ecasb, with staged payment possible after the purchase order is issued
- The final price and delivery time are set in the supplier's formal quotation
- Both parties' contact details are shown once the deal reaches the permitted stage
Ask short questions directly in the messenger; for an official price and proforma, post an RFQ.